Thermal Properties |
Strain Point (°C) |
StP |
|
Annealing Point (°C) |
AP |
|
Transformation Temperature (°C) |
Tg |
426 |
Yield Point (°C) |
At |
456 |
Softening Point (°C) |
SP |
|
Expansion Coefficient  |
-30~+70°C |
145 |
+100~+300°C |
169 |
Thermal Conductivity
 |
k |
0.857 |
Mechanical Properties |
Young's Modulus
 |
E |
691 |
Rigidity Modulus
 |
G |
265 |
| Poisson's Ratio |
|
0.303 |
| Knoop Hardness |
Hk |
320 [3] |
| Abrasion |
Aa |
451 |
Photoelastic Constant
 |
|
0.57 |
|
Chemical Properties |
| Water Resistance (P) |
RW(P) |
1 |
| Acid Resistance (P) |
RA(P) |
3 |
| Weathering Resistance (S) |
W(S) |
3 |
| Acid Resistance (S) |
SR |
52.3 |
| Phosphate Resistance |
PR |
4.3 |
| P = Powder Group, S = Surface Group |
Other Properties |
| Bubble Quality Group |
B |
1 |
| Specific Gravity |
d |
3.62 |
| Coloring |
|
33 |
|
|
28 |
| |
|
Internal Transmittance |
|
|
|
280 |
0.040 |
|
290 |
0.120 |
|
300 |
0.280 |
|
310 |
0.510 |
|
320 |
0.710 |
|
330 |
0.850 |
|
340 |
0.928 |
|
350 |
0.967 |
|
360 |
0.985 |
|
365 |
|
|
370 |
0.992 |
|
380 |
0.996 |
|
390 |
0.997 |
|
400 |
0.996 |
|
420 |
0.995 |
|
440 |
0.995 |
|
460 |
0.996 |
|
480 |
0.997 |
|
500 |
0.998 |
|
550 |
0.999 |
|
600 |
0.998 |
|
650 |
0.997 |
|
700 |
0.998 |
|
800 |
0.998 |
|
900 |
0.997 |
|
1000 |
0.997 |
|
1200 |
0.998 |
|
1400 |
0.998 |
|
1600 |
0.998 |
|
1800 |
0.998 |
|
2000 |
0.998 |
|
2200 |
0.997 |
|
2400 |
0.998 |
|
|